Manufacturing Technology 2023, 23(1):127-134 | DOI: 10.21062/mft.2023.008
Surface Analysis and Digitization of Components Manufactured by SLM and ADAM Additive Technologies
- 1 Department of Machining and Production Engineering, Faculty of Mechanical Engineering - University of Žilina 1, 010 26, Žilina, SLOVAKIA
- 2 Faculty of Mechanical Engineering, Jan Evangelista Purkyne University in Usti nad Labem, Pasteurova 3334/7, 400 01 Usti nad Labem. Czech Republic
The presented article focuses on the surface analysis of the components manufactured by different additive technologies and their reverse digitization. Sintered components were manufactured by SLM and ADAM technologies, while their surface was analyzed using a progressive optical measurement method. To examine the possibility of reverse engineering, the components were optically scanned with a laser scanner and compared to their CAD model. Based on empirical experience, to scan opti-cally the metal and lustrous surfaces is a challenge. The components were manufactured from anti-corrosion materials 17-4 PH and 316L–0407.
Keywords: Additive manufacturing, Sintering, Optical scanning, 17-4 PH, 316L-0407, SLM, Surface texture
Grants and funding:
This article was funded by the University of Žilina project 313011ASY4 – “Strategic implementation of additive technologies to strengthen the intervention capacities of emergencies caused by the COVID-19 pandemic"
Received: January 17, 2023; Revised: March 29, 2023; Accepted: April 6, 2023; Prepublished online: April 24, 2023; Published: May 3, 2023 Show citation
| ACS | AIP | APA | ASA | Harvard | Chicago | Chicago Notes | IEEE | ISO690 | MLA | NLM | Turabian | Vancouver |
References
- TRIMECH. (2022). A Brief History of Additive Manufacturing. In: TriMech Blog [online]: https://blog.trimech.com/a-brief-history-of-additive-manufacturing
- WILLIAMS, J.D, DECKARD, C.R. (1998). Advances in modeling the effects of selected parameters on the SLS process. In: Rapid Prototyping Journal, Vol. 4 No. 2, pp. 90-100.
Go to original source... - HUBS. (2022). Metal 3D printing, [online]: https://www.hubs.com/guides/metal-3d-printing
- LEE, H.; LIM, C.H.J.; LOW, M.J.; THAM, N.; MURUKESHAN, V.M.; KIM, Y.-J. (2017). Lasers in additive manufacturing, In: Int. J. Precis. Eng. Manuf. Green Technol, No. 4, pp. 307-322.
Go to original source... - TIMKO, P., CZÁNOVÁ, T., CZÁN, A., SLABEJOVÁ, S., HOLUBJAK, J. & CEDZO, M. (2022). Analysis of Parameters of Sintered Metal Components Created by ADAM and SLM Technologies. In: Manufacturing Technology, 22, 347-55.
Go to original source... - SAADLAOUI, Y.; MILAN, J.-L.; ROSSI, J.-M.; CHABRAND, P. (2017). Topology optimization and additive manufacturing. Comparison of conception methods using industrial codes. In: J. Manuf. Syst., No. 43, pp. 178-186.
Go to original source... - WOHLERS, T. (2017). Desktop Metal: A Rising Star of Metal AM Targets Speed, Cost and High-Volume Production. Metal AM. Available [online]:
- http://www.metal-am.com/wp-content/uploads/sites/4/2017/06/MAGAZINEMetal-AM-Summer-2017-PDF-sp.pdf
- [8] CHUA, CHEE KAI, LEONG, KAH FAI. (2017). 3D printing and additive manufacturing: principles and applications. In: World Scientific, 5th ed. Singapure, s. 426.
Go to original source... - [9] SLOTA, J., et al. (2013). The Sensitivity of a Photogrammetric Method in Formability Analysis. In: Acta Mechanic et Automatica. Vol. 7, No. 2, ISSN 1898-4088, p. 117-123.
Go to original source... - [10] KOVÁČ, M., BABJAK, Š. (2004). Rapid prototyping - znalostná báza pre projekt laboratória rýchlej prípra-vy výroby. Research report. Košice: Inovačné centrum automobilovej výroby SjF TU v Košiciach, s. 53.
- [11] ALI, H., YERBOLAT, G. & ABILGAZIYEV, A. (2020). Modeling and Simulation of Composite Materials for SLS-Based 3D Printing. In: Manufacturing Technology, 20, 135-42.
Go to original source... - [12] KRUTH, J.-P., B. VANDENBROUCKE, J. VAN VAERENBERGH a P. MERCELIS. (2005). Benchmarking of different SLS/SLM processes as rapid manufacturing techniques. s. 525, [online]: http://doc.utwente.nl/52902/1/Wa1021.pdf
- [13] BURGEROVA, K. & HERMAN, A. (2020). The issue of regeneration of metal powder DLMS 3D printing. In: Manufacturing Technology, 20, 11-7.
Go to original source... - [14] RENISHAW (2021). RenAM 500 metal additive manufacturing (3D printing) systems. In: Renishaw Products, [online]. https://www.renishaw.com/en/renam-500-metal-additive-manufacturing-3d-printing-systems--37011
- [15] RENISHAW. (2021). SS 316L - 0407 Stainless Steel , In: Renishaw Resource centre, [online]; https://tech-labs.com/sites/images/renishaw/data-sheets/H-5800-3001-01-A_SS_316L-0407_material_data_sheet.pdf
- [16] GALATI, M., MINETOLA, P. (2019). Analysis of Density, Roughness, and Accuracy of the Atomic Diffusion Additive Manufacturing (ADAM) Process for Metal Parts. In: MDPI Materials.
Go to original source... - [17] MARKFORGED. (2022). Markforged Metal X, In: Device Datasheet, Markforged [online]; https://s3.amazonaws.com/mf.product.doc.images/Datasheets/2021-docs-folder/F-PR-5000-gen2.pdf
- [18] MARKFORGED. (2022). 17-4 PH Stainless Steel. In: Material Datasheet , Markforged, [online]; https://static.markforged.com/downloads/17-4-ph-stainless-steel.pdf
- [19] DRBÚL, M., ŠAJGALÍK, M., DANIŠ, I. (2019). Povrchové inžinierstvo - 1. vyd. - Žilina: Žilinská univerzita v Žiline, s. 134 [10,93AH]. - ISBN 978-80-554-1566-6
- [20] ALWAID. (2022). 3D laserový skener Aquilon. [online]; https://www.alwaid.cz/aquilon/
This is an open access article distributed under the terms of the Attribution-NonCommercial 4.0 International License (CC BY-NC 4.0), which permits non-comercial use, distribution, and reproduction in any medium, provided the original publication is properly cited. No use, distribution or reproduction is permitted which does not comply with these terms.



ORCID...